Li2TiO3 pebble preparation by extrusion spheronization and sintering process for fusion blanket application

Authors

  • Meghavi Parmar Dept.of Mechanical Engineering (M.E,Production),AITS,Rajkot
  • Aroh Shrivastava Institute for Plasma Research, Gandhinagar Gujarat INDIA
  • Hardik.A.Patel Dept.of Mechanical Engineering (M.E,Production),AITS,Rajkot

Keywords:

-

Abstract

India is developing β-Li2TiO3 Lithium Titanate at Institute for Plasma Research. Lithium titanate will be kept inside the
canisters of TBM (Test Blanket Module) in International thermonuclear experimental reactor (ITER) in form of spherical
pebble bed. Typical size range of these pebbles would be ~ 1 mm. Lithium titanate (Li2TiO3) ceramic powder development is
currently on-going by the solid state reaction process. Reactant material is calcined at (500oC 600oC 700 oC 800oC 900 oC
1000 oC 1050 oC 1100 oC and 1150oC) at 4 hr, 8hr and 12hr. the optimization of solid state reaction is carried out by XRD(Xray Diffraction), and Li2TiO3 Powder has been prepared at 1000oC 4hr.further lithium titanate powder is passed through the
process of ceramic extrusion –spheronization-Sintering of ceramics to Prepare spherical Pebble. At every stage of powder and
pebble preparation extensive characterization has been carried out. Several physical and mechanical properties are
characterized. Sintering parameters of the Li2TiO3 pebbles are also optimized. Surface morphology study of Li2TiO3 pebbles
are also discussed in this paper

Published

2016-06-25

How to Cite

Meghavi Parmar, Aroh Shrivastava, & Hardik.A.Patel. (2016). Li2TiO3 pebble preparation by extrusion spheronization and sintering process for fusion blanket application. International Journal of Advance Research in Engineering, Science & Technology, 3(6), 322–325. Retrieved from https://ijarest.org/index.php/ijarest/article/view/832